Nanoindenter
- Bruker Hysitron TI 950
- Central Research Facility (CRF), Indian Institute of Technology Ropar, Rupnagar
Rates
| Measurement | External academic / Govt | Industry |
|---|---|---|
| per hour | ₹1,000 | ₹2,000 |
- External academic / Govt
- External Academic / Govt. R&D Labs
- Industry
- Industry
Rates from www.iitrpr.ac.in (opens in a new tab). Last checked 2026-11-05. Confirm with the facility before you plan work.
About the facility
- Campus
- Main campus, CRF, IIT Ropar, Rupnagar, Punjab, PIN 140001
- Open to
- Other academic institutes, Government R&D, Industry
- GST
- Extra
Facility page (opens in a new tab)Price list (opens in a new tab)Map
Also at this facility
All 20 instruments- Atomic Force Microscope (SPM/AFM)Bruker Multimode 8 SPM
Atomic Force Microscopyfrom ₹1,000 - Dual-chamber sputtering systemAPT Custom designed
Physical Vapour Deposition, Sputter Coatingfrom ₹3,200 - Field emission SEMJEOL JSM 7610F Plus
Field Emission Scanning Electron Microscopy, Field Emission Scanning Electron Microscopy-Energy Dispersive Spectroscopyfrom ₹1,000 - High-resolution TEM with probe correctorThermo Scientific Themis 300
High-Resolution Transmission Electron Microscopy, Scanning Transmission Electron Microscopyfrom ₹200 - High-resolution mass spectrometer (Q-TOF)Waters Xevo G2-XS QTof
Electrospray Ionization Mass Spectrometry, High-Resolution Mass Spectrometry, Liquid Chromatography-Mass Spectrometryfrom ₹350 - High-temperature furnaceNabertherm RHTH 120/600/18
High-Temperature Furnacefrom ₹110